Experiment Research on Slurry Setting Time’s Effect on High-sulphur Backfill’s Compressive Strength

LAN Zhipeng,WANG Xinmin,WANG Hongjiang,CHEN Qiusong   

  1. School of Resources and Safety Engineering,Central South University,Changsha    410083,Hunan,China
  • Received:2015-12-30 Revised:2016-02-18 Online:2016-10-28 Published:2016-12-27

Abstract:

To explore the relationship between slurry setting time and compressive strength of high-sulphur backfill,an laboratory experiment was carried out,on the basis of tailing’s sulfur content is 25%.The experimental data was analyzed by Origin mathematical software,and the internal microstructure of high-sulphur backfill was observed through SEM.The change law of high-sulphur’s compressive strength in the different condition of slurry setting time was studied.The results show that there is a function relationship between the slurry setting time with different age’s compressive strength of high-sulphur,which bases on the reasonable range of setting time.When the setting time shortened by 15.49%,the early strength increased by 136.17%,but the long-term strength decreased by 19.63%.On the contrary,when the setting time extended by 9.8%,the long-term strength increased by 40.48%,and the long-term strength’s growth pattern was similar to index type.The essence of reducing lost of high-sulphur’s long-term strength is to ensure the uniformity of the microstructure.The research results of this paper can provide reference for high-sulphur mine’s filling work.

Key words: high-sulphur tailings, additives, setting time, compressive strength

CLC Number: 

  • TD853 

[1]  韩鹏,牛桂芝.中国硫矿主要矿集区及其资源潜力探讨[J].化工矿产地质,2010,32(2):95-104.
[2] 翟永刚,吴爱祥,王洪江,等.全尾砂膏体充填临界质量分数[J].北京科技大学学报,2011,33(7):795-799.
[3] 刘同有.充填采矿技术与应用[M].北京:冶金工业出版社,2001.
[4] 王新民,胡一波,王石,等.超细全尾砂充填配比优化正交试验研究[J].黄金科学技术,2015,23(3):45-49.
[5] 刘殿华,吴贤振.全尾砂充填技术的应用与发展[J].世界有色金属,2012(8):44-45.
[6] 蔡嗣经.充填采矿技术的应用现状及发展方向[J].国外金属矿山,1998(6):25-32.
[7] 徐静,杨晓军,徐修平,等.新型固化剂对铜矿全尾砂充填体抗压强度的影响[J].金属矿山,2016(8):190-193.
[8] 刘允秋,侯大德.含硫尾砂充填体强度试验[J].现代矿业,2013(11):195-196.
[9] 王怀勇,张爱民,贺茂坤.高硫极细全尾砂充填料配比及输送特性试验研究[J].中国矿山工程,2014,43(6):1-4.
[10] 王宝,张虎元,董兴玲,等.硫化物氧化对充填体长期强度的影响[J].化工矿物与加工,2007(10):29-31.
[11] 张钦礼,王新民,田明华.硫化物对充填体强度的影响[J].矿业研究与开发,2004,24(增):168-169.
[12] 许毓海.尾砂中硫化物对充填体质量影响研究[J].矿业研究与开发,2009,29(5):4-6.
[13] Ayora C,Chinchon S,Aguado A,et al.Weathering of iron sulfides and concrete alteration:Thermodynamic model and observation in dams from Central Pyrenees,Spain[J].Cement and Concrete Research,1998,28(4):591-603.
[14] Kesimal A,Yilmaz E,Ercikdi B.Evaluation of paste backfill mixtures consisting of sulphide-rich mill tailings and varying cement contents[J].Cement and Concrete Research,2004,34(10):1817-1822.
[15] 张钦礼,康虔,肖富国,等.含硫高粘性尾矿胶结充填关键技术[J].金属矿山,2010(11):39-42,67.
[16] 张钦礼,王新民,古德生,等.新桥硫铁矿粉煤灰充填技术研究[C]//第八届国际充填采矿会议论文集.北京:中国有色金属学会,2004.
[17] 刘海霞.高性能混凝土性能研究及工程应用[D].济南:山东大学,2010.
[18] 肖丽,王新海,盛兴跃.缓凝剂对水泥混凝土性能影响的试验研究[J].公路交通技术,2007(2):25-28.
[19] 张述雄,王栋民,张力冉,等.一种新型无碱液态速凝剂的研究[J].硅酸盐通报,2014,33(11):2946-2951.
[20] 周妍,许文龙,黎学润,等.柠檬酸对阿利特—硫铝酸盐水泥凝结时间及水化过程的影响[J].混凝土,2014(12):76-79.
[21] 中国国家质量监督检验检疫总局.水泥标准稠度用水量、凝结时间,安定性检验方法:GB/1346-2011[S].北京:中国标准出版社,2011.
[22] 潘志华,程建坤.水泥速凝剂研究现状及发展方向[J].建井技术,2005(2):22-27.
[23] 徐群.非线性回归分析的方法研究[D]. 合肥:合肥工业大学,2009.
[24] Benzaazoua M,Belem T,Bussiere B.Chemical factors that influence the performance of mine sulphidic paste backfill[J].Cement and Concrete Research,2002,32(7):1133-1144.

[1] SHI Caixing, GUO Lijie, LI Wenchen, ZHANG Dan. Study on Filling Cementitious Materials Based on Lead-Zinc Smelting Slag and Its Application [J]. Gold Science and Technology, 2018, 26(2): 160-169.
[2] DING Jianfeng. Research on the Ore Bunker Treatment of a Gold Mine [J]. Gold Science and Technology, 2017, 25(4): 52-57.
[3] LI Zongnan,GUO Lijie,YU Bin,SHI Caixing. Shearing Thinning Behavior of High Concentration Slurry Based on Bingham Model [J]. Gold Science and Technology, 2017, 25(4): 33-38.
[4] WANG Xinmin,RONG Shuai,ZHAO Maoyang,ZHANG Qinli . Concentration Equipment Optimization Based on Variable Weight Theory and TOPSIS [J]. Gold Science and Technology, 2017, 25(3): 77-83.
[5] XU Huaihao,LI Jinyou. Application Practice of Increasing Production and Reducing Consumption in Grinding System of Dayingezhuang Gold Mine [J]. Gold Science and Technology, 2017, 25(3): 116-120.
[6] HU Jianhua,YANG Chun,ZHOU Bingren,ZHOU Keping,ZHANG Shaoguo. Simulation of Fracture Propagation and Optimization of Parameters for Smooth Blasting of Coping in Roadway [J]. Gold Science and Technology, 2017, 25(2): 45-53.
[7] JIA Mintao,WANG Qunfang,WU Lengjun. Research Status and Prospect of Thermal Environmental Control Technology Under Deep Mining [J]. Gold Science and Technology, 2017, 25(2): 83-88.
[8] DAI Xingguo,LI Yan,ZHANG Bixiao. Numerical Investigation of Depressurization Full-pipe Transportation of Paste in Deep Mine [J]. Gold Science and Technology, 2016, 24(3): 70-75.
Viewed
Full text


Abstract

Cited

  Shared   
  Discussed   
No Suggested Reading articles found!