摘要:
为提高某高铜含砷金精矿的浸出效果,对碱预处理时间与石灰用量、磨矿细度、浸出速度等主要因素进行一系列的探索试验。结果表明,石灰与碱钠10∶1配合预处理16~14 h, 矿浆浓度33%~35%,CN- 浓度为(0.9~1.2)×10-5 ,磨矿细度-320目90%, 浸出48 h能取得较好的效果。
关键词: 高铜含砷金精矿, 氰化, 预处理, 河台金矿, 广东省
Abstract:
In order to improve the leaching effect of a high-copper gold concentrate containing arsenic,we made a series of exploratory experiment about alkaline pretreatment time,lime dosage,grinding fineness,the leaching rate and other major factors.The results shown that we pretreat lime and alkali sodium with 10:1 for 16~14 hours,when the pulp concentration is 33%~35%,CN-comcentration is(0.9~1.2)×10-5,grinding fineness of-320 mesh 90%,than leached them for 48 hours,could achieve better effect.
Key words: Gold concentrate containing arsenic, Cyanide, Pretreatment, Hetai gold deposit, Guangdong Province
凌育亮. 广东某高铜含砷金精矿处理工艺的试验研究[J]. J4, 2010, 18(2): 61-62.
LING Yo-Liang. Experimetal Study of the Treatment Process about High-copper Gold Concentrate Containing Arsenic[J]. J4, 2010, 18(2): 61-62.